Orthodontic Brackets

正畸托槽
  • 文章类型: Journal Article
    这项研究的目的有三个方面。首先,介绍并详细介绍了一种化学蚀刻不锈钢正畸托槽底座的新方法。其次,该研究试图调查与喷砂基底相比,化学蚀刻后支架内微观结构的结构变化,使用电子显微镜分析。最后,该研究旨在评估和比较具有化学蚀刻底座的正畸托槽与具有喷砂底座的正畸托槽的长期耐久性和生存能力,两者都使用传统的酸蚀刻技术与TransbondXT粘合剂粘合,在18个月的随访期间。
    该研究是一项随机对照试验,采用三重盲法和裂口研究设计,由两组组成。喷砂组中的托架是通过用50μm的SiO2颗粒对托架底部的凹版表面进行喷砂来制备的。使用氢氟酸使酸蚀刻组中的碱粗糙化。在电子显微镜下观察支架的底部以分析地形变化。
    总共5,803个括号(3,006酸蚀,对310名患者进行了2797次喷砂)的粘合,在一个分口设计由同一个操作员。随访18个月。在酸蚀和喷砂组中,故障率分别为2.59%和2.7%,分别。Kaplan-Meier图中的曲线非常接近,两组生存分布在log-rank(Mantel-Cox)检验中无统计学意义;x2=0.062(P值=0.804)。
    如果支架的底部可以用作喷砂的替代方案,则酸蚀刻可以在椅子侧进行。
    UNASSIGNED: The aim of this study was threefold. Firstly, it aimed to introduce and detail a novel method for chemically etching the bases of stainless-steel orthodontic brackets. Secondly, the study sought to investigate the structural alterations within the brackets\' microstructure following chemical etching compared to those with sandblasted bases, using electron microscopy analysis. Lastly, the study aimed to evaluate and compare the long-term durability and survivability of orthodontic brackets with chemically etched bases versus those with sandblasted bases, both bonded using the conventional acid etch technique with Transbond XT adhesive, over an 18-month follow-up period.
    UNASSIGNED: The study was a randomized clinical control trial with triple blinding and split-mouth study design and consisted of two groups. The brackets in the sandblasted group were prepared by sandblasting the intaglio surface of the base of the bracket with 50 µm SiO2 particles. Hydrofluoric acid was used to roughen the base in the acid-etched group. The bases of the brackets were viewed under an electron microscope to analyze the topographical changes.
    UNASSIGNED: A total of 5,803 brackets (3,006 acid-etch, 2,797 sandblasted) in 310 patients were bonded, in a split-mouth design by the same operator. The patients were followed for 18 months. The failure rate of 2.59% and 2.7% was noted in an acid-etched and sandblasted group, respectively. There was a close approximation of curves in the Kaplan-Meier plot, and the survival distribution of the two groups in the log-rank (Mantel-Cox) test was insignificant; x2 = 0.062 (P value = 0.804).
    UNASSIGNED: Acid etching if the bases of the brackets can be used as an alternative to sandblasting furthermore acid etching can be performed on the chair side.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    背景:近年来,使用矫正器进行正畸治疗的需求增加了,由病人的需要,因为对准器通常为它们提供改进的美学和更少的身体不适。在与患者一起决定适当的正畸系统时,重要的是要考虑到潜在的不适和患者对治疗的看法。这项研究的目的是分析支架或矫正器对治疗第一个月的成年患者样本中口腔健康相关生活质量(OHRQoL)和焦虑水平的影响。
    方法:试点研究于2023年11月至2024年2月在萨拉曼卡大学牙科诊所进行。选择了80名开始正畸治疗的成年患者,并将其分为两组:托槽组(Victory®;3MUnitek,加州,美国)(n=40)和对准器组(Invisalign®;对准技术,加州,美国)(n=40)。OHRQoL使用口腔健康影响概况-14(OHIP-14)问卷进行分析,使用状态特质焦虑量表(STAI)分析焦虑。随访时间为一个月,在开始(T0)和开始治疗后一个月(T1)记录评分。
    结果:患者平均年龄为33.70(±5.45)岁。总样本(n=80)包括66.2%的男性和33.8%的女性。在括号组中,开始治疗一个月后,影响最大的维度是身体疼痛(5.62±1.51)。在校准器组中,其中心理残疾维度得分最高(4.22±1.02)。在支架组中,OHIP总评分在1个月(T1)(33.98±6.81)高于治疗开始时(T0)(21.80±3.34);在开始治疗后一个月,未观察到对OHRQoL的更大影响(T1=27.33±6.83;T0=27.33±6.22)。使用的正畸系统不影响参与者的焦虑(p>0.05)。年龄和性别不是OHRQoL和焦虑的影响因素。
    结论:支架系统显著影响患者OHRQoL。在研究的样本中,未观察到正畸系统(托槽与矫正器)对焦虑的影响。
    BACKGROUND: In recent years, the demand for orthodontic treatment with aligners has increased, led by patient need, as aligners typically provide them with improved aesthetics and less physical discomfort. In deciding with the patient on an appropriate orthodontic system, it is important to take into account the potential discomfort and the perceptions that patients have in relation to their treatment. The objective of this study was to analyze the influence of brackets or aligners on oral health-related quality of life (OHRQoL) and anxiety levels in a sample of adult patients during the first month of treatment.
    METHODS: The pilot study was carried out at the Dental Clinic of the University of Salamanca between November 2023 and February 2024. Eighty adult patients who initiated orthodontic treatment were selected and divided into two groups: the brackets group (Victory®; 3 M Unitek, California, USA) (n = 40) and the aligners group (Invisalign®; Align Technology, California, USA) (n = 40). OHRQoL was analyzed using the Oral Health Impact Profile-14 (OHIP-14) questionnaire, and anxiety was analyzed using the State-Trait Anxiety Inventory (STAI). The follow-up time was one month, with scores recorded at the beginning (T0) and one month after starting treatment (T1).
    RESULTS: The mean patient age was 33.70 (± 5.45) years old. The total sample (n = 80) consisted of 66.2% men and 33.8% women. In the brackets group, one month after starting treatment, the dimension with the highest impact was that of physical pain (5.62 ± 1.51). In the aligners group, where the dimension of psychological disability had the highest score (4.22 ± 1.02). In the brackets group the total OHIP score was higher at one month (T1) (33.98 ± 6.81) than at the start of treatment (T0) (21.80 ± 3.34); this greater impact on OHRQoL one month after starting treatment was not observed in the aligners group (T1 = 27.33 ± 6.83; T0 = 27.33 ± 6.22). The orthodontic system used did not influence participants\' anxiety (p > 0.05). Age and sex were not influential factors in either OHRQoL or anxiety.
    CONCLUSIONS: The bracket system significantly influenced patients\' OHRQoL. In the sample studied, no influence of the orthodontic system (brackets versus aligners) on anxiety was observed.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    背景:正畸治疗过程中常见的情况是正畸托槽粘结失败。这项研究调查了基于Er:YAG激光从金属和陶瓷支架的底座上去除粘合剂以进行重新粘合的影响。
    方法:从患者中收集168颗前磨牙。在第1、2、3和4组中,使用84个金属托槽粘合在前磨牙的颊表面上,而在第1组中应用了84个陶瓷托槽,II,III和IV。组1/I代表初始键合基团,第2/II组是带有新括号的重新结合组,而第3/III组和第4/IV组分别接受Er:YAG激光或火焰处理的回收支架。使用通用试验机在所有样品中进行第一和第二脱粘,以确定剪切粘结强度(SBS)。使用立体显微镜评价粘合剂残留指数(ARI)。使用扫描电子显微镜(SEM)评估新的和处理过的托槽底座。通过单向方差分析了初始键合和重新键合能力的差异,ARI的差异用Kruskal-Wallis检验进行评估.
    结果:在激光处理的陶瓷托槽上观察到更大量的粘合剂残留物。第3组(26.13MPa)的回收金属支架的SBS值与第1组(23.62MPa)相当,而与第4组(12.54MPa)则有显着差异。当使用陶瓷托槽比较4组时,没有观察到这些值的显著差异。第4组ARI评分(2~3分)与其他3组比较差异有统计学意义(P<0.05)。对于第一组,II,III和IV,ARI评分相似(P>0.05).SEM分析未显示由Er:YAG激光处理的金属或陶瓷材料组成的支架底座明显损坏。
    结论:Er:YAG激光治疗作为一种去除粘合剂而不损坏支架的方法,优于火焰治疗。Er:YAG激光治疗后的SBS值和ARI评分与新支架相似,为Er:YAG激光治疗提供进一步的支持,作为回收脱粘支架的可行手段。
    BACKGROUND: Failure of orthodontic bracket bonds is a common occurrence during orthodontic treatment. This study investigated the impact of Er: YAG laser-based removal of adhesive from the bases of metal and ceramic brackets for re-bonding.
    METHODS: A total of 168 extracted premolars were collected from patients. 84 metal brackets were used to be bonded on the buccal surface of the premolars in Groups 1, 2, 3 and 4, while 84 ceramic brackets were applied in Groups I, II, III and IV. Group 1/I represented the initial bonding group, with Group 2/II being the re-bonding group with new brackets, while Groups 3/III and 4/ IV received recycled brackets treated by Er: YAG laser or flaming respectively. Both the first and second de-bonding were performed in all samples using a universal testing machine to determine the shear bond strength (SBS). The adhesive remnant index (ARI) was evaluated using a stereo-microscope. The new and the treated bracket bases were evaluated using scanning electron microscopy (SEM). Differences in initial bonding and re-bonding ability were analyzed through one-way ANOVAs, and differences in ARI were assessed with the Kruskal-Wallis test.
    RESULTS: Greater amounts of adhesive residue were observed on ceramic brackets treated by laser. The SBS values for recycled metal brackets in Group 3 (26.13 MPa) were comparable to Group 1 (23.62 MPa) whereas they differed significantly from Group 4 (12.54 MPa). No significant differences in these values were observed when comparing the 4 groups with ceramic brackets. ARI score in Group 4 (2-3 points) differed significantly from the three other groups (P < 0.05). For Group I, II, III and IV, similar ARI scores were observed (P > 0.05). SEM analysis didn\'t show apparent damage of bracket bases consisting of either metal or ceramic material treated by Er: YAG laser.
    CONCLUSIONS: Er: YAG laser treatment was superior to flame treatment as a means of removing adhesive without damaging the brackets. SBS values and ARI scores following Er: YAG laser treatment were similar to those for new brackets, offering further support for Er: YAG laser treatment as a viable means of recycling debonded brackets.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    使用实验支架设计评估牙釉质粘合能力和正畸粘合剂树脂的转化程度。材料和方法。研究中使用了13颗牛齿。对实验支架进行了修改,在其主体的中心有一个半透明区域。搪瓷蚀刻后,正畸正畸粘合剂(FGM,Joinville,巴西)应用在支架底座上进行粘接。将各组划分如下(每组n=10):(1)具有标准支架的对照(CB)和(2)具有实验支架的点支架(SB),其在中心使用碳化物钻具有0.8mm的半透明区域。剪切粘结强度(SBS)在24小时后在万能试验机和粘合剂剩余指数(ARI)中评价。使用拉曼光谱(n=3/组)分析转化程度(DC)。然后使用Studentt检验和Mann-Whitney统计方法分析数据。
    与CB组(8.77MPa)相比,SB组表现出更高的平均SBS(10.33MPa)。然而,组间无统计学差异(p=0.376)。SB组和CB组的平均ARI得分为1分。拉曼分析显示,与CB组(25.9%)相比,SB组(49.3%)的转化率更高。
    实验支持物显示出更高的粘合剂转化率,虽然粘结强度没有显著增加。
    UNASSIGNED: To evaluate the enamel bonding ability and orthodontic adhesive resin degree of conversion using the experimental bracket design. Material and Methods. Thirteen bovine teeth were used in the study. The experimental bracket was modified with a translucent region in the center of its body. After enamel etching, Orthocem orthodontic adhesive (FGM, Joinville, Brazil) was applied on the bracket base for bonding. The groups were divided as follows (n = 10 per group): (1) control (CB) with standard brackets and (2) spot bracket (SB) with experimental brackets featuring a 0.8 mm translucent region at the center using carbide bur. Shear bond strength (SBS) was evaluated after 24 hours in a universal testing machine and adhesive remnant index (ARI). The degree of conversion (DC) was analyzed using Raman spectroscopy (n = 3 per group). Data were then analyzed using Student\'s t-test and Mann-Whitney statistical methods.
    UNASSIGNED: The SB group exhibited a higher mean SBS (10.33 MPa) compared to the CB Group (8.77 MPa). However, there was no statistical difference between the groups (p = 0.376). Both SB and CB groups had a mean ARI score of 1. Raman analysis revealed a higher degree of conversion in the SB group (49.3%) compared to the CB group (25.9%).
    UNASSIGNED: The experimental support showed a higher degree of adhesive conversion, although there was no significant increase in bond strength.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    用金属和金属氧化物的组合或混合对正畸托槽进行纳米涂层可以减少接受固定正畸治疗的患者在托槽周围可见的变形链球菌计数和牙釉质脱钙的发生率。总的来说,255正畸托槽(3MUnitek,蒙罗维亚,加州,USA)分为一个对照组(I组)60和三个实验组65(II组,III,andIV).实验组托槽涂有银氧化锌的组合,氧化铜-氧化锌,和银-铜氧化物纳米颗粒采用物理气相沉积法。用于每组的两种纳米颗粒以1:1的重量比混合,以提供均匀的混合涂层。每组60个支架用于微生物学评估在血琼脂培养基中对变异链球菌的抗菌活性,每个实验组的其余五个支架用于SEM分析,以检查涂层的均匀性。纳米涂层支架表现出比未涂层支架更好的抗菌性能。氧化铜-氧化锌纳米颗粒涂覆的托槽表现出比银-氧化锌和银-氧化铜涂覆的托槽更好的抗菌性能。
    Nano-coating of orthodontic brackets with a combination or hybrid of metals and metal oxides may reduce the streptococcus mutans count and incidence of enamel decalcification seen around brackets in patients undergoing fixed orthodontic treatment. In total, 255 orthodontic brackets (3M Unitek, Monrovia, California, USA) were divided into one control group (group I) of 60 and three experimental groups of 65 each (groups II, III, and IV). The experimental group brackets were coated with a combination of silver-zinc oxide, copper oxide -zinc oxide, and silver-copper oxide nanoparticles using physical vapour deposition method. The two nanoparticles used for each group were mixed in the ratio of 1:1 by weight for providing a uniform hybrid coating. Sixty brackets from each group were used for microbiological evaluation of antibacterial activity against Streptococcus mutans in blood agar medium, and the remaining five brackets from each experimental group were used for SEM analysis to check the uniformity of the coating. Nano-coated brackets demonstrated better antibacterial properties than uncoated brackets. Copper oxide-zinc oxide nanoparticles coated brackets demonstrated better antibacterial properties than the silver-zinc oxide and silver- copper oxide coated brackets.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    背景:金属和弹性体结扎线广泛用于正畸学以将弓丝固定在托槽槽内,但是传统上,弹性结扎线与微生物定植增加有关,这可能会对牙周健康产生不利影响。
    目的:本系统综述比较了用于正畸固定矫治器的弹性体结扎线和钢结扎线对牙周的影响。
    方法:7个数据库的无限制文献检索(MEDLINE,Scopus,WebofScience,Embase,Cochrane系统评价数据库,Cochrane中央控制试验登记册,和虚拟健康图书馆),直到2023年7月,对人类进行了随机/非随机临床研究,比较了固定矫治器治疗期间的两种结扎方法。重复研究选择后,数据提取,和偏倚风险评估与风险偏倚(RoB)2或非随机研究中的偏倚风险-干预(ROBINS-I)工具,进行了平均差异(MD)或标准化平均差异(SMD)及其95%置信区间(CI)的随机效应荟萃分析,然后用建议等级评估现有证据的确定性,评估,发展,和评估(等级)方法。
    结果:共纳入11项研究(3项随机/8项非随机),其中354例患者(平均年龄14.7岁,42%为男性)。菌斑指数无统计学差异(5项研究;SMD=0.48;95%CI=-0.03至1.00;P=0.07),牙龈指数(2项研究;MD=0.01;95%CI=-0.14至0.16;P=0.89),探测口袋深度(2项研究;MD=0;95%CI=-0.17至0.16;P=0.97),或变形链球菌计数(4项研究;SMD=0.40;95%CI=-0.41至1.20;P=0.21)。弹性结扎线与细菌总负荷适度增加相关(3项研究;SMD=0.43;95%CI=0.10至0.76;P=0.03)。在所有情况下,由于纳入了具有高偏倚风险的非随机研究,对这些估计的信心都很低。
    结论:现有的低质量证据表明,在固定治疗期间,结扎方法似乎不会影响牙周健康,即使弹性结扎线与细菌负荷的适度增加有关。
    背景:PROSPERO(CRD42023444383)。
    BACKGROUND: Metallic and elastomeric ligatures are widely used in orthodontics to secure the archwire within the bracket slots, but elastomeric ligatures have traditionally been associated with increased microbial colonization, which could adversely affect periodontal health.
    OBJECTIVE: This systematic review compares the periodontal effects of elastomeric and steel ligatures used for orthodontic fixed appliances.
    METHODS: Unrestricted literature search of 7 databases (MEDLINE, Scopus, Web of Science, Embase, Cochrane Database of Systematic Reviews, Cochrane Central Register of Controlled Trials, and Virtual Health Library) up to July 2023 were performed for randomized / non-randomized clinical studies on humans comparing the two ligation methods during fixed-appliance therapy. After duplicate study selection, data extraction, and risk-of-bias assessment with the Risk of Bias (RoB) 2 or the Risk Of Bias In Non-randomized Studies - of Interventions (ROBINS-I) tool, random-effects meta-analyses of Mean Differences (MD) or Standardized Mean Differences (SMD) and their 95% confidence intervals (CIs) were carried out, followed by assessment of certainty of existing evidence with the Grades of Recommendation, Assessment, Development, and Evaluation (GRADE) approach.
    RESULTS: A total of 11 studies (3 randomized / 8 non-randomized) with 354 patients (mean age 14.7 years and 42% male) were included. No statistically significant differences were seen for plaque index (5 studies; SMD = 0.48; 95% CI = -0.03 to 1.00; P = 0.07), gingival index (2 studies; MD = 0.01; 95% CI = -0.14 to 0.16; P = 0.89), probing pocket depth (2 studies; MD = 0; 95% CI = -0.17 to 0.16; P = 0.97), or Streptococcus mutans counts (4 studies; SMD = 0.40; 95% CI=-0.41 to 1.20; P = 0.21). Elastomeric ligatures were associated with moderately increased total bacterial load (3 studies; SMD = 0.43; 95% CI = 0.10 to 0.76; P = 0.03). Confidence in these estimates was low in all instances due to the inclusion of non-randomized studies with high risk of bias.
    CONCLUSIONS: Existing low quality evidence indicates that ligature method does not seem to influence the periodontal health during fixed treatment, even if elastomeric ligatures are associated with a moderate increase of bacterial load.
    BACKGROUND: PROSPERO (CRD42023444383).
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    背景:研究50%抗坏血酸与50%柠檬酸溶液对牙齿漂白后金属支架的即时剪切粘结强度(SBS)的影响。还测定了35%过氧化氢(HP)漂白后的釉质蚀刻图案和作为抗氧化剂的这些组合酸的所需量。
    方法:以各种时间间隔评估溶液在室温下的稳定性。将50颗牙齿随机分为五组:非漂白(G1),漂白,然后酸蚀(G2),漂白,然后用10%抗坏血酸钠和酸蚀(G3)处理10分钟,用50%抗坏血酸(G4)处理5分钟,和用50%抗坏血酸和50%柠檬酸(G5)的组合处理5分钟。组G2、G3、G4和G5用35%HP凝胶漂白总共32分钟。使用37%磷酸(Ormco®,橙色,CA,美国)15秒。在所有组中,立即使用Transbond™XT底漆和Transbond™PLUS粘合剂粘合金属支架,光固化40秒。SBS用万能试验机进行了测试,采用单因素方差分析和Tukey'sHSD检验进行统计学分析。所有统计检验的显著性水平设定为p<0.05。
    结果:稳定性测试表明组合的酸保持有效长达21天。G5组显著提高漂白牙齿的SBS至G1水平(p<0.05),而G3的SBS没有达到相同的增加(p>0.05)。SEM分析显示牙釉质蚀刻图案与两个对照组(G1和G2)相似。6分钟时的动力学研究表明,G5中的抗氧化反应比G3和G4中的抗氧化反应低0.2mmol。
    结论:与未漂白的牙齿相比,联合酸的5分钟应用可增强漂白牙齿的SBS。合并的酸在两周内保持稳定,提出了一个省时的,在正畸托槽粘接中应用抗氧化剂和牙釉质蚀刻的单步解决方案。
    BACKGROUND: To investigate the effect of a 50% ascorbic acid with 50% citric acid solution on the immediate shear bond strength (SBS) of metallic brackets after tooth bleaching. The enamel etching pattern and the required quantity of these combined acids as antioxidants following 35% hydrogen peroxide (HP) bleaching were also determined.
    METHODS: The stability of the solution at room temperature was assessed at various time intervals. Fifty teeth were randomly divided into five groups: non-bleached (G1), bleached then acid etched (G2), bleached followed by a 10-minute treatment with 10% sodium ascorbate and acid etched (G3), 5-minute treatment with 50% ascorbic acid (G4), and 5-minute treatment with a combination of 50% ascorbic acid and 50% citric acid (G5). Groups G2, G3, G4 and G5 were bleached by 35% HP gel for a total of 32 min. Acid etching in groups G1, G2, and G3 was performed using 37% phosphoric acid (Ormco®, Orange, CA, USA) for 15 s. In all groups, metal brackets were immediately bonded using Transbond™ XT primer and Transbond™ PLUS adhesive, with light curing for 40 s. The SBS was tested with a universal testing machine, and statistical analysis was conducted using one-way ANOVA followed by Tukey\'s HSD test. The level of significance was set at p < 0.05 for all statistical tests.
    RESULTS: Stability tests demonstrated that the combined acids remained effective for up to 21 days. Group G5 significantly increased the SBS of bleached teeth to the level of G1 (p < 0.05), while G3 did not achieve the same increase in SBS (p > 0.05). SEM analysis revealed enamel etching patterns similar to those of both control groups (G1 and G2). Kinetic studies at 6 min indicated that the antioxidation in G5 reacted 0.2 mmole lower than in G3 and G4.
    CONCLUSIONS: 5-minute application of the combined acids enhanced the SBS of bleached teeth comparable to unbleached teeth. The combined acids remain stable over two weeks, presenting a time-efficient, single-step solution for antioxidant application and enamel etching in orthodontic bracket bonding.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    正畸托槽上各种微生物的大量生长可形成斑块并引起疾病。为正畸不锈钢罐(SST)开发了一种新型的胺封端的超支化锆-聚硅氧烷(HPZP)抗菌涂层。合成HPZP和HPZP-Ag涂层后,它们的结构通过核磁共振波谱来表征,扫描电子显微镜,厚度测量,接触角检测,机械稳定性测试,和腐蚀测试。通过细胞计数试剂盒八种测定法检测两种涂层对人牙龈成纤维细胞(hGFs)和人口腔角质形成细胞(hOKs)的细胞毒性,和SST,HPZP@SST,HPZP-Ag@SST与金黄色葡萄球菌共培养,大肠杆菌,和变形链球菌24小时,以检测涂层的抗菌性能,分别。结果表明,涂层厚度约为10μm,HPZP涂层的水接触角显著高于HPZP-Ag涂层(P<0.01)。两种涂层均能在SST上均匀、致密地分布,具有良好的机械稳定性和耐腐蚀性。细胞计数试验表明,HPZP涂层和HPZP-Ag涂层对细胞的毒性较SST小,HPZP-Ag涂层的毒性大于HPZP涂层,与hGF和hOK共培养72小时后,细胞存活率大于80%。抗菌试验表明,不同材料表面的细菌数量由小到大依次排列:HPZP@SST The massive growth of various microorganisms on the orthodontic bracket can form plaques and cause diseases. A novel amine-terminated hyperbranched zirconium-polysiloxane (HPZP) antimicrobial coating was developed for an orthodontic stainless steel tank (SST). After synthesizing HPZP and HPZP-Ag coatings, their structures were characterized by nuclear magnetic resonance spectroscopy, scanning electron microscopy, thickness measurement, contact angle detection, mechanical stability testing, and corrosion testing. The cell toxicity of the two coatings to human gingival fibroblasts (hGFs) and human oral keratinocytes (hOKs) was detected by cell counting kit eight assays, and SST, HPZP@SST, and HPZP-Ag@SST were cocultured with Staphylococcus aureus, Escherichia coli, and Streptococcus mutans for 24 hr to detect the antibacterial properties of the coatings, respectively. The results show that the coatings are about 10 μm, and the water contact angle of HPZP coating is significantly higher than that of HPZP-Ag coating (P < 0.01). Both coatings can be uniformly and densely distributed on SST and have good mechanical stability and corrosion resistance. The cell counting test showed that HPZP coating and HPZP-Ag coating were less toxic to cells compared with SST, and the toxicity of HPZP-Ag coating was greater than that of HPZP coating, with the cell survival rate greater than 80% after 72 hr cocultured with hGFs and hOKs. The antibacterial test showed that the number of bacteria on the surface of different materials was ranked from small to large: HPZP@SST < HPZP-Ag@SST < SST and 800 μg/mL HPZP@SST showed a better bactericidal ability than 400 μg/mL after cocultured with S. aureus, E. coli, and S. mutans, respectively (all P < 0.05). The results showed that HPZP coating had a better effect than HPZP-Ag coating, with effective antibacterial and biocompatible properties, which had the potential to be applied in orthodontic process management.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Systematic Review
    正畸治疗,虽然对于实现最佳口腔健康至关重要,由于正畸矫治器上细菌粘附和生物膜形成的倾向,在感染控制方面面临挑战。镀银正畸材料已经成为一种有前途的解决方案,利用银纳米颗粒(AgNPs)的有效抗菌性能。在正畸中使用抗菌涂层来防止细菌生物膜的形成。这篇系统的综述评估了固定正畸矫治器上抗菌银涂层的文献,包括弓丝,括号,和微植入物。两名评估人员,独立工作,严格对各种数据库进行全面搜索,包括PubMed,PubMedCentral,Embase,Scopus和WebofScience本系统综述全面检查了体外研究,研究了镀银正畸弓丝的抗菌功效,括号,和微植入物。PROSPEROCRD42024509189中注册的评论综合了18项不同研究的结果,揭示细菌粘附的一致和显著减少,生物膜的形成,和菌落计数与AgNP的掺入。关键研究证明了银涂层弓丝和托槽对常见口腔细菌的有效性,如变形链球菌和金黄色葡萄球菌。涂覆有AgNP的微植入物还表现出对一系列微生物的显著抗微生物活性。系统评价揭示了这些抗菌作用的潜在机制,强调了正畸实践中预防感染的意义,并提出了未来的研究途径。尽管有一些研究的异质性和局限性,集体证据支持镀银正畸材料在减轻细菌并发症方面的潜力,强调它们在推进正畸感染控制措施中的相关性。
    Orthodontic treatments, while essential for achieving optimal oral health, present challenges in infection control due to the propensity for bacterial adhesion and biofilm formation on orthodontic appliances. Silver-coated orthodontic materials have emerged as a promising solution, leveraging the potent antimicrobial properties of silver nanoparticles (AgNPs). Antibacterial coatings are used in orthodontics to prevent the formation of bacterial biofilms. This systematic review evaluated the literature on antimicrobial silver coatings on fixed orthodontic appliances, including archwires, brackets, and microimplants. Two evaluators, working independently, rigorously conducted a comprehensive search of various databases, including PubMed, PubMed Central, Embase, Scopus and Web of Science. This systematic review comprehensively examined in vitro studies investigating the antimicrobial efficacy of silver-coated orthodontic archwires, brackets, and microimplants. The review registered in PROSPERO CRD42024509189 synthesized findings from 18 diverse studies, revealing consistent and significant reductions in bacterial adhesion, biofilm formation, and colony counts with the incorporation of AgNPs. Key studies demonstrated the effectiveness of silver-coated archwires and brackets against common oral bacteria, such as Streptococcus mutans and Staphylococcus aureus. Microimplants coated with AgNPs also exhibited notable antimicrobial activity against a range of microorganisms. The systematic review revealed potential mechanisms underlying these antimicrobial effects, highlighted implications for infection prevention in orthodontic practice, and suggested future research avenues. Despite some study heterogeneity and limitations, the collective evidence supports the potential of silver-coated orthodontic materials in mitigating bacterial complications, emphasizing their relevance in advancing infection control measures in orthodontics.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

  • 文章类型: Journal Article
    背景:白点的形成,代表早期龋齿病变,是固定正畸的一个主要问题。向正畸粘合剂中添加再矿化剂可以防止白点的形成。这项研究的目的是生产一种复合正畸粘合剂结合纳米生物活性玻璃-银(nBG@Ag)用于支架粘结牙釉质,并研究其细胞毒性,抗菌活性,再矿化能力,和粘结强度。
    方法:使用溶胶-凝胶法合成nBG@Ag,并使用透射电子显微镜(TEM)进行表征,X射线衍射(XRD)和傅里叶变换红外光谱与衰减全反射附件(ATR-FTIR)。含1%胶粘剂的细胞毒性试验(MTT)和抗菌活性,3%,和5%(wt/wt)nBG@Ag进行评估,使用万能试验机测量粘合剂的剪切粘合强度。通过使用维氏显微硬度计和扫描电子显微镜(SEM)的显微硬度测试来评估再矿化。使用Shapiro-Wilk检验进行统计分析,平衡试验,单向方差分析,Robust-Welch试验,TukeyHSD方法,和双向方差分析。
    结果:发现粘合剂的生物相容性很高,如样品组和对照组之间的细胞毒性没有显着差异所证实的。由含有nBG@Ag的复合材料制成的圆盘显示变形链球菌的生长显着降低(p<0.05),抗菌活性随着nBG@Ag百分比的增加而增加。添加纳米粒子后,粘合剂的剪切粘合强度显着下降(p<0.001),但仍高于建议值。nBG@Ag的添加显示出牙齿显微硬度的改善,尽管研究组之间的显微硬度差异无统计学意义.通过SEM和能量色散X射线光谱(EDX)确认了牙齿表面上羟基磷灰石沉积物的形成。
    结论:在正畸粘合剂中添加nBG@Ag可以是增强抗菌活性和减少正畸托槽周围牙釉质脱矿的有效方法,不损害生物相容性和粘结强度。
    BACKGROUND: The formation of white spots, which represent early carious lesions, is a major issue with fixed orthodontics. The addition of remineralizing agents to orthodontic adhesives may prevent the formation of white spots. The aim of this study was to produce a composite orthodontic adhesive combined with nano-bioactive glass-silver (nBG@Ag) for bracket bonding to enamel and to investigate its cytotoxicity, antimicrobial activity, remineralization capability, and bond strength.
    METHODS: nBG@Ag was synthesized using the sol-gel method, and characterized using transmission electron microscopy (TEM), X-ray diffraction (XRD), and Fourier-transform infrared spectroscopy with an attenuated total reflectance attachment (ATR-FTIR). The cytotoxicity test (MTT) and antimicrobial activity of adhesives containing 1%, 3%, and 5% (wt/wt) nBG@Ag were evaluated, and the shear bond strength of the adhesives was measured using a universal testing machine. Remineralization was assessed through microhardness testing with a Vickers microhardness tester and scanning electron microscopy (SEM). Statistical analyses were conducted using the Shapiro-Wilk test, Levene test, one-way ANOVA, Robust-Welch test, Tukey HSD method, and two-way ANOVA.
    RESULTS: The biocompatibility of the adhesives was found to be high, as confirmed by the lack of significant differences in the cytotoxicity between the sample and control groups. Discs made from composites containing nBG@Ag exhibited a significant reduction in the growth of Streptococcus mutans (p < 0.05), and the antibacterial activity increased with higher percentages of nBG@Ag. The shear bond strength of the adhesives decreased significantly (p < 0.001) after the addition of nanoparticles, but it remained above the recommended value. The addition of nBG@Ag showed improvement in the microhardness of the teeth, although the differences in microhardness between the study groups were not statistically significant. The formation of hydroxyapatite deposits on the tooth surface was confirmed through SEM and energy-dispersive X-ray spectroscopy (EDX).
    CONCLUSIONS: Adding nBG@Ag to orthodontic adhesives can be an effective approach to enhance antimicrobial activity and reduce enamel demineralization around the orthodontic brackets, without compromising biocompatibility and bond strength.
    导出

    更多引用

    收藏

    翻译标题摘要

    我要上传

       PDF(Pubmed)

公众号